    Cutting too many corners, and now burnt.
     
  3. warejon9

    warejon9 What's a Dremel?

    Joined:
    20 Apr 2010
    Posts:
    165
    Likes Received:
    2
    This started cropping up on XS a while ago, glad they're getting it sorted, hopefully mine should be ok as not using feser fluid.
     
  4. p0Pe

    p0Pe gief cake?

    Joined:
    23 Nov 2007
    Posts:
    1,442
    Likes Received:
    94
    I find it funny how this is only happening to EK´s waterblocks, and still they blame the coolant :D
    Harden the frack up EK...
     
  5. p0Pe

    p0Pe gief cake?

    Joined:
    23 Nov 2007
    Posts:
    1,442
    Likes Received:
    94
    warejon9,
    This problem have nothing to do with the fluid used. It is solely based on sub-par nickel plating, and cutting corners in manufacturing as rickysio also stated.
     
  6. Jaybles

    Jaybles Minimodder

    Joined:
    12 Feb 2011
    Posts:
    981
    Likes Received:
    54
    They never tried to blame the coolant, they are saying that the additives or silver coils are causing THEIR nickel plating to corrode. They are not trying to blame another product otherwise they wouldn't have stopped production, and they wouldn't be trying to fix it. They are also offering a full warranty for the corrosion. I fail to see how they are fobbing this off on someone else.
     
  7. p0Pe

    p0Pe gief cake?

    Joined:
    23 Nov 2007
    Posts:
    1,442
    Likes Received:
    94
    Kindly explain this statement then:
    http://farm4.static.flickr.com/3271/5800743334_6aee97c96c_o.jpg

    "nickel is nickel" right?

    Many times EK stated that their was NOTHING wrong with their nickel plating, and even in the "official" test they trew out, it was only mentioned that "the fluid is eating away the nickel"
    Not once did EK suspect that their plating process was the issue, and kept trying to blame everything else.

    It is the exactly same story as with their cracking and leaking reservoirs. Just more stuff is affected this time.

    And about the production stop, they should have done that loooong time ago. It was only after sidewindercomputers stopped selling their blocks duo to the test made on rrtech that EK manned up.
     
  8. Jaybles

    Jaybles Minimodder

    Joined:
    12 Feb 2011
    Posts:
    981
    Likes Received:
    54
    Apologies, i wasn't aware the issue had been going on that long.
     
  9. KayinBlack

    KayinBlack Unrepentant Savage

    Joined:
    2 Jul 2004
    Posts:
    5,913
    Likes Received:
    533
    It's what I'd do.

    I lost an EK Supreme HF as well as the entire loop attached to it from flaking nickel pounded through the loop. The whole deal was a loss.

    However, I still have a copper 470 block I have no intentions of replacing. Picked myself up a Kryos Pro on sale at Sidewinder to replace the EK. Mine was old enough it was not covered by the RMA.
     
  10. p0Pe

    p0Pe gief cake?

    Joined:
    23 Nov 2007
    Posts:
    1,442
    Likes Received:
    94
    Kayin, your not gonna regret getting a Kryos ;) I have both the delrin and the XT version and they rock!
     
  11. (FIH) The Don

    (FIH) The Don What's a Dremel?

    Joined:
    27 Jun 2010
    Posts:
    76
    Likes Received:
    0
    if they dont get this fixed now, it will definately cause some massive damage on EK's not too good rep



    imho
     
  12. Angel OD

    Angel OD Pump Killer

    Joined:
    16 Sep 2007
    Posts:
    1,610
    Likes Received:
    114
    (FIH) The Don <- The problem has been ongoing for so long that their rep is toast... In my book at least!
    And that's a damn shame! I personally believe that they made huge mistakes trying to blame everything but their nickelplater...
     
  13. rjkoneill

    rjkoneill What's a Dremel?

    Joined:
    11 Feb 2008
    Posts:
    280
    Likes Received:
    6
    ek nickel in my system for a good year now.
    no signs of corrosion but then, i dont use additives. just plain old distilled and a little mayhems dye.
     
  14. Phil Rhodes

    Phil Rhodes Hypernobber

    Joined:
    27 Jul 2006
    Posts:
    1,415
    Likes Received:
    10
    Really good electroplating is extremely complicated.

    What, if anything, are they putting between the nickel and the copper?
     
  15. Floyd

    Floyd Wire Twister

    Joined:
    4 Dec 2008
    Posts:
    288
    Likes Received:
    1
    Cmon EK, I have some older FC 275 blocks and they are just fine with distilled and a silver coil. Sounds like the new blocks plating is just junk.
    Rubidium is a great guy that really knows his stuff.
     
  16. Pete J

    Pete J Employed scum

    Joined:
    28 Sep 2009
    Posts:
    7,258
    Likes Received:
    1,824
    Heh, nickel 'corrosion'.

    Deposition method needs looking at IMHO.
     
  17. Shayper09

    Shayper09 Swimming in Deionized.

    Joined:
    14 Jun 2010
    Posts:
    128
    Likes Received:
    0
    Bugger! I have a 580 nickel block with a kill coil, ho
     
  18. Shayper09

    Shayper09 Swimming in Deionized.

    Joined:
    14 Jun 2010
    Posts:
    128
    Likes Received:
    0
    Bugger! I have a 580 nickel block with a kill coil, hopefully won't be an issue! :(
     
  19. Fat Tony

    Fat Tony Minimodder

    Joined:
    3 Jul 2009
    Posts:
    375
    Likes Received:
    15
    Err - how do I tell if I have a problem ?

    (2 x Nickel Plated 580 blocks)
     
  20. sixfootsideburns

    sixfootsideburns modeteer

    Joined:
    6 Feb 2009
    Posts:
    618
    Likes Received:
    9
    they're so full of ****... it has nothing to do with the coolant, they're plating process just shat the bed that's all
     